I am investigating the possibility plating foam (Syntatic foam) with Al. and was wondering if anybody has had any luck doing so. The plating must encapsulate the entire piece which includes holes completely through the foam ( average hole ~ 1” dia.). The size of the foam sheet can vary but first look is 20.0" X 10" X 2.0".
Also, any thoughts on CTE mismatch of such a "composite" looking at delta T of 45 C...will the foam conform with the plating as it grows or will the foam tear away at the edges?
Do I treat the CTE calculation of the Al. plating the same way as solid Al. plate?
Any websites or alternative process would be appreciated!
Also, any thoughts on CTE mismatch of such a "composite" looking at delta T of 45 C...will the foam conform with the plating as it grows or will the foam tear away at the edges?
Do I treat the CTE calculation of the Al. plating the same way as solid Al. plate?
Any websites or alternative process would be appreciated!