Dear Sirs,
I'm talking about a Client Specification that requires an NPS 30 pipe to be manufactured as per A672 C60 Class 32 (i.e. Normalized) and, in addition, this pipe shall be made from a plate as per ASTM A516 GR60 Normalized!!
Practically my Client asks for a double normalization heat treatment, on plate first and then on pipe after welding. I find this choice to be quite odd, do you agree? What's your experience about? Did it ever happened to apply a double normalisation heat treatment? What risks may I occur? (My first concern is that no Vendor would supply such an Item!)
For the sake of clarity, I specify that I'm in HIC service, 248HV on HAZ and 200HB on weld deposit (practically NACE MR0103 but not explicitly mentioned).
Thank you for your attention, I hope for a reply of yours.
Regards,
ES
I'm talking about a Client Specification that requires an NPS 30 pipe to be manufactured as per A672 C60 Class 32 (i.e. Normalized) and, in addition, this pipe shall be made from a plate as per ASTM A516 GR60 Normalized!!
Practically my Client asks for a double normalization heat treatment, on plate first and then on pipe after welding. I find this choice to be quite odd, do you agree? What's your experience about? Did it ever happened to apply a double normalisation heat treatment? What risks may I occur? (My first concern is that no Vendor would supply such an Item!)
For the sake of clarity, I specify that I'm in HIC service, 248HV on HAZ and 200HB on weld deposit (practically NACE MR0103 but not explicitly mentioned).
Thank you for your attention, I hope for a reply of yours.
Regards,
ES