Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Plastic Strain Data for Steel and PTFE

Status
Not open for further replies.

bogiedreamer

Mechanical
Joined
Apr 14, 2005
Messages
57
Is there a material data library in Abaqus? I need plastic strain data for Steel and PTFE.

I found this steel data from an Abaqus tutorial from a University, could anyone verify that it is correct?

*ELASTIC
210.E09, 0.31

*PLASTIC
200.2E06, 0.0
246.0E06, 0.0235
294.0E06, 0.0474
374.0E06, 0.0935
437.0E06, 0.1377
480.0E06, 0.18
 
If your units are Pascals, then it is probably correct. You should be careful about blinding using material data...
 
I agree with vumat721 - you need to be careful about defining your material, as it is as important as the mesh and boundary conditions in correctly defining a model.

Also, what sort of steel are you trying to model? The yield stress of steel can vary widely from low carbon (~400 MPa) right up to the highly alloyed steels (~1400 MPa).

Regards



Martin Stokes CEng MIMechE
 