He,

I have a question for you all. Does somebody know if there is a plastic that is thermoformable and resistant to IPA and PGMEA. IPA is some kind of alcohol and PGMEA is some kind of ether.

If somebody can let me know it would be great!

Thanks,

Roy van Zanten
Ajax Custom Plastics
 
PGMEA is Propylene Glycol Monomethyl Ether Acetate.

IPA is IsoPropyl Alcohol.

HDPE will work for IPA, I don't know about PGMEA.

Regards,

Cory