I am designing a plastic cover with a latch and plastic hinge. Is there any online documentation or share ware describing design concepts for snap fits and plastic hinges?
 
meh70us,

This topic, at least in part, was covered in prior threads. Try the thread thread288-34812: Plastic snap fits on cylindrical components. Try also searching on Google.com.

Best regards,

Matthew Ian Loew

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora
 
If you get the CD ROM from Bayer Plastics, it contains a lot of very comprehensive design documents in PDF format, one of which covers the design of latches in plastic.
 
I designed a similar part a couple years ago. Polypropylene is your best material for a living hinge, although I have heard of people using polyethylene and nylon.

Try GE plastics. You will need to register and get a password.

Here is their design guide for living hinges

And here is thei guide for snap fits.

Like Biggadike said, Bayer Plastics has some good info on Snap fits:

Dow has some info on living hinges here:


Efunda has some good stuff too:
 