, Automotive Division (formerly GE Plastics). Some discussions I've had with them opened my eyes to some very interesting plastics they are targeting to "under the hood" applications.
TygerDawg
Blue Technik LLC
Virtuoso Robotics Engineering
Sabic don't have nylon and this is very likely a nylon application.
In my experience while GE (now Sabic) has some very good materials there representatives where extremely partisan to the extent that much of what they said had to be questioned. I certainly had to where possible, clean up a lot of their messes over here. One recommendation was so bad that three boat anchors (failed moulds) was enough for a multinational to close down their manufacturing here and fire about 700 people. Another two where so bad that product launches where delayed for over 12 months while alternate materials where tried and moulds reworked to accommodate.
Regards
Pat