hello, i`m having a problem with a plastic container we manufacture and its cap. the container (300 mL)is PP made by blowmolding. the problem consist in a overlap when I apply some force to the cap. i checked the diameters of the container screw and are the same of another container with diferent form, capacity(600 mL) and dimensions which use the same cap.