What is considered to be Pitting Corrosion and what are the main causes/factors that determine it in CS heat exchanger tubes? In turn, what are the answers to these questions for the case of Uniform or General Corrosion?

Thanks!
 
Replies continue below

Recommended for you

It's a matter of terminonology and definitions, and what you consider as 'Uniform or General Corrosion'.
Refer to API RP 571 which provides a soudn basis for this. There, youll see pitting is a form corrosion. General or uniform corrosion (of carbon steel) is mentioned under Cooling Water Corrosion (sect 4.3.4).
 