Hello all..
I am having some parts anodized that will be deployed in saltwater for years. Recently have seen pitting. The pitting does not cover the entire surface of the part. Mainly seen in the ridges and grooves. Any suggestions? Also, can a part show up from the anodizer with no pits and within days they begin to form?
Here are the instructions for the anodizer..
Anodize per MIL-A-8625, Rev F, Type III, Class 1, Duplex Seal (Sodium Dichromate first, nickel acetate second soak)
Build up: 0.00075" per side
Thanks all..
SandyH
I am having some parts anodized that will be deployed in saltwater for years. Recently have seen pitting. The pitting does not cover the entire surface of the part. Mainly seen in the ridges and grooves. Any suggestions? Also, can a part show up from the anodizer with no pits and within days they begin to form?
Here are the instructions for the anodizer..
Anodize per MIL-A-8625, Rev F, Type III, Class 1, Duplex Seal (Sodium Dichromate first, nickel acetate second soak)
Build up: 0.00075" per side
Thanks all..