Hello friends,
We have an SS304 shell. there are tubes in it (like shell & tube heat exchangers). in the shell we have cooling water. We found pitting on bottom welds of the shell and the leakage of water. perhaps it was because of chloride content of water. we test the water and it has more than 800 ppm chloride.
We used belzona but the leakage continued (maybe because of wrong usage)
What is your suggestion for repair of the shell and stopping the pitting?
Do you know when the base material may affect by pitting seriously?
Consider that there are some problems :
1- We dont have access to inside of the shell.
2- re-welding may be harmfull because there is gasket behind the weld. and also removing the shell is impossible.
Your help is appreciated.
We have an SS304 shell. there are tubes in it (like shell & tube heat exchangers). in the shell we have cooling water. We found pitting on bottom welds of the shell and the leakage of water. perhaps it was because of chloride content of water. we test the water and it has more than 800 ppm chloride.
We used belzona but the leakage continued (maybe because of wrong usage)
What is your suggestion for repair of the shell and stopping the pitting?
Do you know when the base material may affect by pitting seriously?
Consider that there are some problems :
1- We dont have access to inside of the shell.
2- re-welding may be harmfull because there is gasket behind the weld. and also removing the shell is impossible.
Your help is appreciated.