TugboatEng
Marine/Ocean
- Nov 1, 2015
- 11,825
Who is going to tell them?
I know this is a bit out of place but it seems we all need a refresher on the weaknesses or stainless steel from time to time. I wonder who it was that attached the description of "marine grade" to type 316. I have some strong words for them![[evil] [evil] [evil]](/data/assets/smilies/evil.gif)
The Article said:Stainless steel 316L is a popular choice for marine applications due to its excellent combination of mechanical strength and corrosion resistance.
I know this is a bit out of place but it seems we all need a refresher on the weaknesses or stainless steel from time to time. I wonder who it was that attached the description of "marine grade" to type 316. I have some strong words for them