Need help with lessons learned and potential gotcha's with in plant weld repair methods. Point is to repair and ship as good parts with proper repairs.
Is there a repair standard out there?
1. MIG process
2. 1010 steel
3. 2.5" sheet steel, fillet welded.
In addition, what is key to minimizing weld variation specifically tip changes and tip to work distances. tips are changed frequently.
Is there a repair standard out there?
1. MIG process
2. 1010 steel
3. 2.5" sheet steel, fillet welded.