I would like to find a full updated chart for the maximum
allowable working pressure for welded and threaded carbon
steel pipe (all sizes & schedules) with corrosion factors from 0 CA to 1/4" CA
 
Replies continue below

Recommended for you

Dear Sr
You can consulting the ANSI B31.G You can To calculate the MAOP Or Stress remaining for Deep of pitting or length of corrosion.

Regards
Jorge

jorge@tecnicontrol.com.co
 
I am looking for more information about defect assessment for pipework B31.3.
 
Alloy625 CA
Dear Members
Can anyone help me with corrosion allowances for alloy625 pipes in 250mm and 300mm diameters, both Sch10
Any assistance would be appreciated.