Hello,
Original wall thikness of 28" column overhead line was 10mm. The pipe material is ASTM A 672 GRB60 CL12. After 20 years of operation the inspection has found the wall thickness reduced to 7.8mm and recommends for replacement of the line in next plant Turn Around.
The calculated wall thickness as per ASME B31.3 of the 28" line using design condition is 5.3mm (including 3mm CA).
As the available thickness of pipe is still more than the required thickness as per calculation, can we retain the same line or is there some other points that has to be considered in deciding the action plan. Please suggest.
Thanks
Original wall thikness of 28" column overhead line was 10mm. The pipe material is ASTM A 672 GRB60 CL12. After 20 years of operation the inspection has found the wall thickness reduced to 7.8mm and recommends for replacement of the line in next plant Turn Around.
The calculated wall thickness as per ASME B31.3 of the 28" line using design condition is 5.3mm (including 3mm CA).
As the available thickness of pipe is still more than the required thickness as per calculation, can we retain the same line or is there some other points that has to be considered in deciding the action plan. Please suggest.
Thanks