Dear forum members,
There is a leak (multiple pin holes next to each other) on a 2" line which is heavily corroded (operating pressure 2 bars, oily water).
The line can not be shutdown for a long time (10-15 min), leak is close to U bolt support, surface is very corroded...
Is there some composite material one can stick in / on and it may no need through surface preparation (actually if it can be applied to a oily wet surface) ?
Or what code compliant or non - compliant suggestion might be ?
Thks
There is a leak (multiple pin holes next to each other) on a 2" line which is heavily corroded (operating pressure 2 bars, oily water).
The line can not be shutdown for a long time (10-15 min), leak is close to U bolt support, surface is very corroded...
Is there some composite material one can stick in / on and it may no need through surface preparation (actually if it can be applied to a oily wet surface) ?
Or what code compliant or non - compliant suggestion might be ?
Thks