Hello all,
I am preparing to install a transfer line for a mixed acid. We recieve a mixture of 70% H2SO4, 5% HNO3, balance H2O. Does anybody have a recommendation on material of construction for the pipe?
The temperature will be ambient, pressure will be 30 psig.
Thanks.
I am preparing to install a transfer line for a mixed acid. We recieve a mixture of 70% H2SO4, 5% HNO3, balance H2O. Does anybody have a recommendation on material of construction for the pipe?
The temperature will be ambient, pressure will be 30 psig.
Thanks.