Feb 14, 2009 #1 dursosono Materials Joined Aug 6, 2008 Messages 59 Location ID Does pipe's diameter is essential variable for procedure qualifications per ASME IX?
Feb 14, 2009 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US No, not for procedure qualification. Upvote 0 Downvote
Feb 16, 2009 #3 DVWE Petroleum Joined Apr 5, 2007 Messages 2,374 Location US That is correct. The only limitation is performance qualification (not procedure). See QW-302. Upvote 0 Downvote
Feb 19, 2009 #4 carlomaderazo Mechanical Joined Jan 15, 2005 Messages 56 Location QA According ASME IX, if your welding procedure has been qualified to plate it's qualified to pipe as well. Upvote 0 Downvote
According ASME IX, if your welding procedure has been qualified to plate it's qualified to pipe as well.