Dear all,
Pipelines SS304L will be installed in our plant (classical welding not orbital) for transportation of liquid raw materials ( mineral oils, silicon oils.. ) . So how it should be cleanend after installation because it must be completely clean an dry? Do we need cleaning with phosphoric acid , then deionised water and at the end with (levoxin+hydrohinine)?
BR
Orion
 