Good morning,
I am working with piping company which specialized on only aboveground pipeworks. And there is an upcoming pipeline work that we will possible get awarded.
Our old procedures are outdated, could anyone explain me current pipeline works. I mean is 2-3 group stick SMAW welding still popular?
Should we do Argon GTAW root and then SMAW fill? Work is roughly 100km, will full SMAW be faster? Or is it not worth it due to the better root result with GTAW root.
Thanks,
I am working with piping company which specialized on only aboveground pipeworks. And there is an upcoming pipeline work that we will possible get awarded.
Our old procedures are outdated, could anyone explain me current pipeline works. I mean is 2-3 group stick SMAW welding still popular?
Should we do Argon GTAW root and then SMAW fill? Work is roughly 100km, will full SMAW be faster? Or is it not worth it due to the better root result with GTAW root.
Thanks,