Dear All
Whilst there's strong evidence that pipeline deposits lower the inhibitor concentration and coverage, I am curious to see evidence of field experience supported (not laboratory )corrosion rates for under deposit corrosion under the following :
1. Export Condensate with no threat of MIC (so purely under deposit driven)
2. Combined MIC and under deposit corrosion.
3. Under both scenerio, the velocity of the condensate is low (<1 m/s)

I realise that indeed many other factors come into play, but curios to see any decent published field experience which assumes corrosion rates.

Many thanks
 
NACE Corrosion 2012, Paper 1379 might provide the first stepping stone.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top