I'd to know some experience in restoring cement linning in 8" and 15' OD pipeline on-site(without unburied it) with 3Km (1.86 miles) between manholes.
Thanks
 
Replies continue below

Recommended for you

That is a tough assignment. The lines are too small to get into, so you would need a remote control injection mould device.

Can you put a Polyethylene Pipe inside as a lining? You will need to excavate some temporary manholes for the work.
 