Hi,
I am modelling the indenatation and collapse of a subsea pipeline. The hemispherical indenter is modelled as an analytical rigid surface. The pipeline is modelled resting on a perfectly flat seabed which is also analytical rigid.
The displacement of the indenter is moved downwards until it reaches 1/3 of the pipeline diameter before being incrementally retracted in a seperate step. Both these steps work well with no significant warning messages being shown.
The problems arise when i try to initiate collapse of the pipeline by applying an external pressure to the deformed geometry. I am using STATIC, RIKS for this step. As the pressure is applied the pipeline begins to collapse, forming the figure of 8 shape I would expect to see. However, the pipline never reaches the fully collapsed mode, and the collapse process reverses before the pipeline begins to expand across its cross-section. Not what I am expecting!
Can anyone help me out with this step?
My aim is to understand how the collpase pressure changes with varying dent depth.
Many Thanks
I am modelling the indenatation and collapse of a subsea pipeline. The hemispherical indenter is modelled as an analytical rigid surface. The pipeline is modelled resting on a perfectly flat seabed which is also analytical rigid.
The displacement of the indenter is moved downwards until it reaches 1/3 of the pipeline diameter before being incrementally retracted in a seperate step. Both these steps work well with no significant warning messages being shown.
The problems arise when i try to initiate collapse of the pipeline by applying an external pressure to the deformed geometry. I am using STATIC, RIKS for this step. As the pressure is applied the pipeline begins to collapse, forming the figure of 8 shape I would expect to see. However, the pipline never reaches the fully collapsed mode, and the collapse process reverses before the pipeline begins to expand across its cross-section. Not what I am expecting!
Can anyone help me out with this step?
My aim is to understand how the collpase pressure changes with varying dent depth.
Many Thanks