Jul 30, 2008 #1 vscid Nuclear Joined Aug 5, 2007 Messages 65 Location US What would be the best callout to weld the pipe to the triangular piece? pipe: 300 series stainless, 1.25 OD, 1.125 ID, trinagular plate: 300 series stainless, 0.25 thick. Thanks!
What would be the best callout to weld the pipe to the triangular piece? pipe: 300 series stainless, 1.25 OD, 1.125 ID, trinagular plate: 300 series stainless, 0.25 thick. Thanks!
Jul 30, 2008 #2 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,262 Location JP Do you mean "What is the proper call-out for the parts shown, with no further joint preparation?" or "What would be the best joint for welding these two things together?" If the former, I think it's a flare-bevel. If the later, much more information is needed. Upvote 0 Downvote
Do you mean "What is the proper call-out for the parts shown, with no further joint preparation?" or "What would be the best joint for welding these two things together?" If the former, I think it's a flare-bevel. If the later, much more information is needed.