Hi All,
Do you include pipe tolerance when calculation for internal pressure? If use SA106B pipe, there is 12.5% tolerance on the wall thickness, I think the schedule wall thickness need to be reduced by 12.5% to truly reflect the worse case shell thickness.
If use formula given in UG-27
P=SET/(R+0.6t) where t is schedule thickness times 0.785
Agreed?
So shall we also apply tolerance on the Pipe OD? so for worse case scenario, max OD, with min wall.
BTW, what is the max allowable manufacture under thickness for for A516 70 plate ?
But I found, when using PV Elite, it did not consider any tolerance.
Do you include pipe tolerance when calculation for internal pressure? If use SA106B pipe, there is 12.5% tolerance on the wall thickness, I think the schedule wall thickness need to be reduced by 12.5% to truly reflect the worse case shell thickness.
If use formula given in UG-27
P=SET/(R+0.6t) where t is schedule thickness times 0.785
Agreed?
So shall we also apply tolerance on the Pipe OD? so for worse case scenario, max OD, with min wall.
BTW, what is the max allowable manufacture under thickness for for A516 70 plate ?
But I found, when using PV Elite, it did not consider any tolerance.