Got into a discussion about piping and fatigue. The terms that were thrown around were "Piping", "Tubing" and "Pipe Sized Tubing".
We have a blow pipe (I use pipe because I am not sure what is installed) that snapped due to fatigue. The pipe spans 9 ft, with blow holes every 9". Compressed air is pulsed into the pipe and which is distributed into the holes. (It is a reverse air pulse jet bag house). The movement of the air is causing the pipe to oscillate, then crack at the center hole, eventually it snaps.
Ok, here is where it gets complicated: The shop forman says he used 1 in "piping". Another shop guy says it is 1 in "tubing". The Project manager pulled out a book and said that it is 1 in "pipe sized tubing" and added that it is superior to piping.
I know that pipe is not the same as tube. I've never heard of "pipe size tubing", but that doesn't mean it does not exists. My question is: Is there such a thing a "Pipe sized tubing"? and where can I find data on it?
The solution to the problem was to add a series of brackets a the midpoint to restrict the pipe.
"I drank what?!" Socrates?
We have a blow pipe (I use pipe because I am not sure what is installed) that snapped due to fatigue. The pipe spans 9 ft, with blow holes every 9". Compressed air is pulsed into the pipe and which is distributed into the holes. (It is a reverse air pulse jet bag house). The movement of the air is causing the pipe to oscillate, then crack at the center hole, eventually it snaps.
Ok, here is where it gets complicated: The shop forman says he used 1 in "piping". Another shop guy says it is 1 in "tubing". The Project manager pulled out a book and said that it is 1 in "pipe sized tubing" and added that it is superior to piping.
I know that pipe is not the same as tube. I've never heard of "pipe size tubing", but that doesn't mean it does not exists. My question is: Is there such a thing a "Pipe sized tubing"? and where can I find data on it?
The solution to the problem was to add a series of brackets a the midpoint to restrict the pipe.