Hi, All,
I am looking to find suitable piping material to convey (1) VOC contaminated Groundwater from the subsurface. HDPE is one possibility. However not sure about its reliability in a long term. (2)Another application is conveying high octane number aviation fuel from the subsurface. Can HDPE be used?
How about using PVDF for both applications?
Thanks!
 
Replies continue below

Recommended for you

HDPE is good.

HDPE for oil & gas gathering spec sheet

Corp of Engineers has been using HDPE for landfill gas extraction (ETL 1110-1-160 17 APR 95)


Other VOC remediation techniques in COE TGs, TE, and Engineer Manuals. Hope they are useful to you,

Title: Engineering and Design - Technical Guidelines for Hazardous and Toxic Waste Treatment and Cleanup Activities

Engineering and Design - Multi-Phase Extraction

Process Design Manual for Land Treatment of Municipal Wastewater

EPA references,
**********************
"Pumping accounts for 20% of the world’s energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies)
 
See the regulatory agency document at
Beyond permeation issues and structural property changing and/or weakening warnings etc. noted in this regulatory document (talking about water, sewer, and storm etc. pipelines -- see e.g. , "Once compromised, permeated plastic piping must be replaced since the piping will retain its swollen porous state after permeation and chemical degradation..." etc.), I would only further note that it should also be realized that natural absorption of hydrocarbons into a plastic pipe wall can/will? reportedly also cause other problems e.g. with any future required or desired repair or lateral connections (taps, etc.) involving fusions to the affected pipes (.The site e.g. e.g. now includes the caveat,

"Liquid Hydrocarbon Permeated Pipe
Liquid hydrocarbons such as crude oil, gasoline, kerosene, fuel oil, natural gas condensates and the like that are in the pipe or in surrounding soil will permeate into the pipe wall. Liquid hydrocarbon permeation generally has a minor effect on pipe that is already installed and joined. However, weak, unreliable joints can result when heat fusion is used to join polyolefin piping that has been permeated with liquid hydrocarbons.
In the field, liquid hydrocarbon permeation is indicated by a bubbly or pock-marked surface when the heating tool is removed during fusion joining. In some instances, the odor of the liquid hydrocarbon from the pipe or the surrounding soil or an enlarged pipe OD can be an indication.
Research indicates that joints made using pipes having moderate to higher levels of liquid hydrocarbon permeation will be unreliable, low-strength fusion joints. Low levels of liquid hydrocarbon permeation may not be as deleterious, but there are no quick field tests to determine the actual level of permeation..." )
 