Hi friends, can we weld the pipe line API 5L X60 with the pipe line API 5L X52
Thanks a lot
 
If you're asking this question it is because you require real-person professional assistance.

Short answer: yes.

"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
 