PIPE formed in normalising condition A106B 1

Status
Not open for further replies.

RajanQ

Mechanical
May 15, 2012
4
We are using 26" pipe as shell for H2S stripper vessel. The design requires A106B normalised Pipe. We can only get pipe formed in Normalised condition. Can we use the pipe.
 
Replies continue below

Recommended for you

The formed pipe should be re-normalized to ASTM A 106B material specification to remove all remanent affects from forming.
 