pipe coating

yazguli

Mechanical
Jan 4, 2013
38
Hi everybody!
Would you please help me to understand the terms in the attached image?
Thank you a lot.
 

Attachments

  • Screenshot 2025-01-28 194940.png
    Screenshot 2025-01-28 194940.png
    57.7 KB · Views: 16
Replies continue below

Recommended for you

looks like someone put this through google translate.

It seems to say grit blast to SA 2.5, then primer coat of 40 micron, followed by top coat of 60 micron, total 100 micron thick.

Possibly with some sort of cut back on the ends or a cap protecting the ends / inside the pipe.
 
Thank you very much, LittleInch. And sorry to be so late to read your answer.
 