Hi All,
I am new in the piping design world, and I was asked to design a spool with a hydrotest package for a gas line operating at 1,200 psi at a north region in Canada.
I choose the following materials for the spool:
· The pipe can be a NPS 1 XS A-106 (WT 0.133 in)
· A NPS 2: NPS 1 reducer made of A-105N
· Weld neck flanges - ANSI 600 – A105N
· A ¾ “ TOR – 3000# - A105N
I did not specify which Category to use I II or III, since I am a bit confused as to what the categories really represent
From what i read on CSA Z662, categories I, II, III represent the notch toughness and different exposed temperatures (I might me wrong).
Therefore, since this spool piece is in a facility and can experience temperatures as low as -45 C, would it be saved to assume that a Category II or Category III pipe is required?
Also, Table 5.3 in CSA Z662 indicates pipe types and their limitations in category, so how come a pipe made out of A-106 is not applicable to Cat II and Cat III applications?
I would really appreciate any advice or comment.
Thank you
I am new in the piping design world, and I was asked to design a spool with a hydrotest package for a gas line operating at 1,200 psi at a north region in Canada.
I choose the following materials for the spool:
· The pipe can be a NPS 1 XS A-106 (WT 0.133 in)
· A NPS 2: NPS 1 reducer made of A-105N
· Weld neck flanges - ANSI 600 – A105N
· A ¾ “ TOR – 3000# - A105N
I did not specify which Category to use I II or III, since I am a bit confused as to what the categories really represent
From what i read on CSA Z662, categories I, II, III represent the notch toughness and different exposed temperatures (I might me wrong).
Therefore, since this spool piece is in a facility and can experience temperatures as low as -45 C, would it be saved to assume that a Category II or Category III pipe is required?
Also, Table 5.3 in CSA Z662 indicates pipe types and their limitations in category, so how come a pipe made out of A-106 is not applicable to Cat II and Cat III applications?
I would really appreciate any advice or comment.
Thank you