Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

pins breaking point

Status
Not open for further replies.

Kurt98

Mechanical
Nov 28, 2006
7

I would like to know how many tons of pressure a .625 pin made of A2 steel could handle before it breaks. If there is a formula i would also like to know it for future reference. Thank you
 
Replies continue below

Recommended for you

It's just the cross-sectional area of the pin (pi x r x r) multiplied by the shear strength of the metal. If it's in double-shear (like a clevis pin), then you can basically double this figure.

Don
Kansas City
 
Kurt98,

If eromlignod did not answer your question then you probably do not know the shear strength. If you still need help, let us know what is the hardness of the A2 or the tempering temperaure one or the other and I think I can find the shear strength in my Tool Steel text or Metals Handbook.

 
What type of a steel A2 is? I am familiar with A36, A55 and the A2XXX series but not A2.
 
A2 is a medium-alloy cold worked tool steel, which uses air as its quenching medium. The temperature range is 1700F-1800F. Tempering temperature is 350F-1000F. The resulting hardness is 62-57 Rc. Hope this helps.
 