j8715
Mechanical
- Apr 29, 2009
- 6
Hi
Currently I have a system from a vendor with a 1.25:1 ratio. The Gear is 84 Hrb and the pinion is around 42 Hrb (I can't really get to it to test it easily, I'm guessing from a material book). No surprise the pinion is failing very quickly. My question is how much harder do I make the pinion for best performance? I have a book that suggests the pinion should be 20 to 70% harder, that seems like an awfully large range. I assume it should be dependent on the ratio of the drive, since the ratio isn't extreme do I stay on the low side, say 20-30% harder?
Thanks
Currently I have a system from a vendor with a 1.25:1 ratio. The Gear is 84 Hrb and the pinion is around 42 Hrb (I can't really get to it to test it easily, I'm guessing from a material book). No surprise the pinion is failing very quickly. My question is how much harder do I make the pinion for best performance? I have a book that suggests the pinion should be 20 to 70% harder, that seems like an awfully large range. I assume it should be dependent on the ratio of the drive, since the ratio isn't extreme do I stay on the low side, say 20-30% harder?
Thanks