I am looking for other potential root cause for pin broken.
After induction hardening, both pin were broken after use.
After counter check the hardness, the hardness range from 52-60hrc.
Will the slightly increasing of hardness cause the pin failure?
any other potential root cause?
Spec:
Material : S45C
Treatment : Induction Hardening (Hardness : 48-52 HRC)