lithography
Electrical
I have a pin hole leak in a hydrogen pipe. The pipe passed near a HCL tank and has corroded. The pipe is 1" steel and the H2 is pressurised to 60psi. I want to make a temporay repair to this pipe and was looking for some ideas from engineers that may have had similar experiences in this type of repair situation. Needles to say this will only be temporay measure while we plan and schedule replacement of old pipe and re-routing.