Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Piercing and Blanking Aluminum Sheet

Status
Not open for further replies.

cobra427

Mechanical
Jan 2, 2003
1
I have a part currently being waterjet cut from sheet stock 3/16" thick. Can anyone enlighten me to the problems we would experience in stamping these parts in a die? we have the press, the technology, and the orders for increasing capacity by stamping versus cutting.
 
Replies continue below

Recommended for you

cobra427,
what material, size, tolerance and quantity required you're looking at?

Best regards,
ct
 
Cobra 427,

my company makes tool steel and one of the biggest problems our customers have with aluminium is cold welding.

We use coatings for this nowadays.