I'll second the last few responses.
It sounds like it's likely a PT slab due to expansive soil and the PT slab was designed for a PI of 32. If PI is less than 15, it's not considered expansive per the IBC. It sounds like the designer is telling the construction side to reach out to them if the PI is less than 15 or on solid rock as it's then not considered expansive and the PT slab is overdesigned; therefore, the slab can be redesigned and will likely be thinner, less reinforcement, cheaper, etc. Good on the designer.