Hello !

I'm facing an issue. I want to disperse photoactive nano-particle in a polymer matrix, but this latter is degradated by UV ? Does someone can help me finding a solution ?

Regards,

Hook
 
I probably can help if you provide reasonable details about your question.

Please don't double post. It wastes time and dilutes input.

It looks better if you red flag one of the posts yourself and save me the effort of doing it for you.



Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Translates to (at a guess): "I am putting TiO2 into a polymer and want to stop it attacking the polymer."

There are well known solutions to that. Most TiO2 is coated in silicate to stop it attacking polymers. Another approach is to use the special doped TiO2 from Oxonica (Tradename Optisol or Solacor). The dopant stops it attacking polymer and also improves its UV adsorbing abilities.

There is not any memory with less satisfaction than the memory of some temptation we resisted.
- James Branch Cabell
 
burndirt

Do you have any conection withNorthern Nano

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top