Hi Guys

I ma looking for the maximum tool steels admitted in Commercial Hot Tool steels grades like H11 & H13

A supplier n°1 sends us a Quotation for H11 hot work Steel with 0.024 %of phosphorus.

A second supplier sends us a quotation with 0.018 % phosphorus but with higher price

The dilemma is what to choose: price or quality level of phosphors ?

I want to need what is the impact of the 2 level of phosphorus 0.024 ù Vs 0.018 %

• UTS
• Yield Strength
• Elongation
• Impact toughness
• Fatigue limit
• the life of the moulds especially at elevated temperature up to 500°C

Your help are welcome

Stanislas

 
Replies continue below

Recommended for you

Always good to go with low P. If P was in 0.010 levels or below, a premium price would have been justified ,but for 0.018%P,is it called fleecing?

_____________________________________
"It's better to die standing than live your whole life on the knees" by Peter Mayle in his book A Good Year
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor