Dear Sirs,
We want to transfer phosphoric acid (70 to 80% strength) through 12" dia stainless steel SS 304L grade pipeline (5km long)@450 tons/hour at 4 to 5 bar pressure.There will be such two transfers of about 2000 tons parcels each in a month.This pipeline will be immediately pigged with suitable pig & washed with water after each transfer is over.I would like to know the compatibility of the pipeline grade with the product & any adverse effect,corossion in the line,effect on pipeline life if any.
Thanks,
dkb
We want to transfer phosphoric acid (70 to 80% strength) through 12" dia stainless steel SS 304L grade pipeline (5km long)@450 tons/hour at 4 to 5 bar pressure.There will be such two transfers of about 2000 tons parcels each in a month.This pipeline will be immediately pigged with suitable pig & washed with water after each transfer is over.I would like to know the compatibility of the pipeline grade with the product & any adverse effect,corossion in the line,effect on pipeline life if any.
Thanks,
dkb