HI:
Can anyone give me a step by step procedure for injecting
phosphate or chemical in boiler water.
Please comment on the following procedure:
1. Add water in mixing tank.
2. Add tri-sodium phosphate solution to tank.
3. Start mixer (motor).
4. Open mixing tank outlet to dosing pump.
5. Start pump and line up phospate to boiler water.
Or should the pump be started on water first and the
phosphate to be added later??
Where can i accurate information on this, are there
any websites or handbooks??
Can anyone give me a step by step procedure for injecting
phosphate or chemical in boiler water.
Please comment on the following procedure:
1. Add water in mixing tank.
2. Add tri-sodium phosphate solution to tank.
3. Start mixer (motor).
4. Open mixing tank outlet to dosing pump.
5. Start pump and line up phospate to boiler water.
Or should the pump be started on water first and the
phosphate to be added later??
Where can i accurate information on this, are there
any websites or handbooks??