Phospating

Status
Not open for further replies.

TitoPri

Mechanical
Joined
Jan 5, 2008
Messages
3
Location
AR
Hi,

Since I am a mcechanical engineer and I have to assist a mn-phosphating line for carbon steel couplings.
It is operating temperature is about 97 degree C.

However, it is need to improve the photphating layer thinkness.

Would like provide the appropriate material to study about this process

Best regards,

 
Contact Heatbath. They are the leader in manganese phosphate in the industry. Or contact your supplier. Have you checked:

Free Acid
Total Acid
Iron Content


ck1999
 
Thanks for your reply.

The plant is operating with Henkel supplies. They are going to visit us the next week, after some claims.

The values are.

Free Acid 1.6
Total Acid 11.5
Iron Content 0.33
 