I may be in the wrong forum, thought I'd start here. We have a few spray pads in our parks. All but a couple are concrete structures. These others have asphalt for the pads. The pads are like a cooling fountain for kids to run around in. The water runs into the drains, into a tank, pumped through filters, treated then pumped out again. (Conservation). The pH is easy to maintain on the concrete pads, however the asphalt pads are very difficult to maintain neutrality, it climbs dramatically, well above 8.5. Should asphalt have this affect?