Hi,
I m refering UG 79 for dish end forming of material SA 240 316 L.
When I refered UHA-44 for heat treatment , u noticed there only 25 grades of stainless steel given in table UHA-44 and SS 316 L not listed in it.
Now what to do ???
It means Heat treatment required for material not listed in table or Not required for them.
Any one have idea about this ???
I will do strain calculation as per UG-79-1 but then what to refer for those material which not listed in UHA 44 table.
 