Strange problem on simulating a pressurized bottle .
On Abaqus/Explicit i'm using the folowings :
1. Density : 1.37E-009 tonne/mm3
2. Young's Modulus : 3100 MPa
3. Internal Pressure Load : 0.4 MPa
Now the strange thing is that I'm having a huge deformation.
In practice with a pressure of 0.4 MPa (4 athmospheres) i have around 0.5-1 mm deformation, but in abaqus the simulation results in a huge deformation and sometimes in errors without any result.
The strangiest part is that if i use 1.37 density (PET density in g/cm3) the results seems to folow the practice.
I'm new to abaqus is there a missed calculation of units or what is wrong ?
On Abaqus/Explicit i'm using the folowings :
1. Density : 1.37E-009 tonne/mm3
2. Young's Modulus : 3100 MPa
3. Internal Pressure Load : 0.4 MPa
Now the strange thing is that I'm having a huge deformation.
In practice with a pressure of 0.4 MPa (4 athmospheres) i have around 0.5-1 mm deformation, but in abaqus the simulation results in a huge deformation and sometimes in errors without any result.
The strangiest part is that if i use 1.37 density (PET density in g/cm3) the results seems to folow the practice.
I'm new to abaqus is there a missed calculation of units or what is wrong ?