I am currently working on the design of a flexible permeable pavement, (first time doing so). The reason to implement this material is to minimize, even eliminate, stormwater runoff.
According to TxDOT, I was able to come up with most variables except the Mr (Resilient Modulus) for the two-layer system.
The in-situ soil is a Sandy Soil (USC Soil Type SM).
I can easily come up with Mr if I were to follow the following equations;
1) Mr = 2555 x (CBR)^0.64
2) Mr = 1500 x (CBR)
The problem I am running into is that I can not get accurate and/or reliable CBR values for (1) No.57 aggregate with 40% void ratio for the reservoir layer and (2) the flexible permeable top layer.
Also, the Mr values do change depending on the Wet and Dry season.
Any guidance related to the change due to wet/dry season would be appreciated.
Thank you so much!
I am currently working on the design of a flexible permeable pavement, (first time doing so). The reason to implement this material is to minimize, even eliminate, stormwater runoff.
According to TxDOT, I was able to come up with most variables except the Mr (Resilient Modulus) for the two-layer system.
The in-situ soil is a Sandy Soil (USC Soil Type SM).
I can easily come up with Mr if I were to follow the following equations;
1) Mr = 2555 x (CBR)^0.64
2) Mr = 1500 x (CBR)
The problem I am running into is that I can not get accurate and/or reliable CBR values for (1) No.57 aggregate with 40% void ratio for the reservoir layer and (2) the flexible permeable top layer.
Also, the Mr values do change depending on the Wet and Dry season.
Any guidance related to the change due to wet/dry season would be appreciated.