Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PEPTOR 3S effect on rubber properties ?

Status
Not open for further replies.

Bhasmang

Chemical
Joined
Aug 8, 2019
Messages
4
Location
IN
can anyone explain what will be the effect of peptor on final rubber propertie.
i know the peptor is used to break chain bonds in natural rubber for easily mixing .
currently i saw a formulation using 500gm of peptor 3s with RSS 3 & SVR 3L .
what will effect if i reduce the peptor dosage to 65gm. maybe because of higher dosage of peptor tread resulting in soft side ?
 
Peptisers are expensive so, it makes complete sense to use as little as possible in order to keep costs down. I would not use SVR3L in any formulation requiring the addition of carbon black because it is intended for use in light coloured compounds.