Anna220284
Mechanical
Hello All,
I have being working on a new design for a helium vessel 316L parent material with welding filler 316LSi. We have carried out the impact Charpy V test for a PQR at 77K following the design standard EN ISO 13445. Following this design standard we strongly believe we comply with PED as it is harmonised standard.
The NOBO is reviewing the WPQR and I have been told we should do the impact test at 4.2k as the minimum operating temperature.
I am getting stressed trying to give them evidence that such low T for impact test it is not required.
13345 clearly states 77K is the required temperature for impact testing for any design operating at <-105°C.
Anyone had similar experience with Notified Body?
I have being working on a new design for a helium vessel 316L parent material with welding filler 316LSi. We have carried out the impact Charpy V test for a PQR at 77K following the design standard EN ISO 13445. Following this design standard we strongly believe we comply with PED as it is harmonised standard.
The NOBO is reviewing the WPQR and I have been told we should do the impact test at 4.2k as the minimum operating temperature.
I am getting stressed trying to give them evidence that such low T for impact test it is not required.
13345 clearly states 77K is the required temperature for impact testing for any design operating at <-105°C.
Anyone had similar experience with Notified Body?