Could anybody share his/her experience on compacting asphalt layers over AASHTO No. 57 aggregate base. Does No. 57 move and prevent pavement from being compacted? Thanks
 
Replies continue below

Recommended for you

Is the 57 stone crushed or round ?
In general a bad idea.
I have found that the pavement can have settlement issues under parked cars the asphalt can push in the the voids in the summer.
 