What is the nominal mix used for C25?
 
Replies continue below

Recommended for you

1:2:4 mix ratio The nominal mix for C25 concrete is a ratio of 1 part cement, 2 parts sand, and 4 parts gravel. This means that for every one bucket of cement, you need two buckets of sand and four buckets of gravel. This mix helps make strong concrete that's great for building.
 