Could someone tell me if I can passivate Nitronic 60, UNS21800, and if so which type I should use from the ASTM-A-967 spec?

Thank you,

Bob
 
Replies continue below

Recommended for you

We standardized on "ASTM-A-967, less sect 12 thru 21".